Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | <= 4700 cP @Temperature 23.0 °C |
<= 4700 cP @Temperature 73.4 °F |
|
Solvay SIPOMER® PAM-200 Phosphate Esters of Ppg Monomethacrylate Description: Sipomer PAM-200 incorporated into acrylic resin systems improves adhesion to metallic substrates and glass. Due to its versatile compatibility characteristics with various common solven.. |