Physical Properties Metric English Comments
Viscosity <= 4700 cP

@Temperature 23.0 °C
<= 4700 cP

@Temperature 73.4 °F
Solvay SIPOMER® PAM-200 Phosphate Esters of Ppg Monomethacrylate
Description: Sipomer PAM-200 incorporated into acrylic resin systems improves adhesion to metallic substrates and glass. Due to its versatile compatibility characteristics with various common solven..