Physical Properties Metric English Comments
Viscosity 461700 cP

@Shear Rate 500 1/s,
Temperature 240 °C
461700 cP

@Shear Rate 500 1/s,
Temperature 464 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..