Viscosity 42.0 - 300000 cP

@Temperature 190 - 230 °C
42.0 - 300000 cP

@Temperature 374 - 446 °F
Average value: 40700 cP Grade Count:13
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Viscosity 42.0 - 300000 cP

@Shear Rate 300 - 5000 1/s
42.0 - 300000 cP

@Shear Rate 300 - 5000 1/s
Average value: 40700 cP Grade Count:13
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..