Polymer Property : Viscosity = 415 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 415 cP

@Temperature 70.0 °C
415 cP

@Temperature 158 °F
BASF Pluracol® 736 Rigid Polyol
Description: Pluracol® 736 polyol is an aromatic initiator-based polyol which can be used in a variety of rigid foam formulations. This polyol can be reacted with crude MDI, crude TDI or TDI quasip..
Viscosity 415 cP

@Temperature 60.0 °C
415 cP

@Temperature 140 °F
BASF Pluracol® 735 Rigid Polyol
Description: Pluracol® 735 polyol is a modifying polyol which can be used in a wide variety of rigid foam applications and can be formulated using crude MDI, crude TDI, or TDI quasi-prepolymers. Fo..