Viscosity 410000 cP

@Shear Rate 500 1/s,
Temperature 205 °C
410000 cP

@Shear Rate 500 1/s,
Temperature 401 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)  (Unverified Data**)
Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det..