DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for coInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ISO 1183
Viscosity 94000 cP

@Shear Rate 5000 1/s,
Temperature 220 °C
94000 cP

@Shear Rate 5000 1/s,
Temperature 428 °F
ISO 11403-1 -2
100000 cP

@Shear Rate 5000 1/s,
Temperature 205 °C
100000 cP

@Shear Rate 5000 1/s,
Temperature 401 °F
ISO 11403-1 -2
108000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
108000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
ISO 11403-1 -2
356000 cP

@Shear Rate 500 1/s,
Temperature 220 °C
356000 cP

@Shear Rate 500 1/s,
Temperature 428 °F
ISO 11403-1 -2
410000 cP

@Shear Rate 500 1/s,
Temperature 205 °C
410000 cP

@Shear Rate 500 1/s,
Temperature 401 °F
ISO 11403-1 -2
471000 cP

@Shear Rate 500 1/s,
Temperature 190 °C
471000 cP

@Shear Rate 500 1/s,
Temperature 374 °F
ISO 11403-1 -2
Linear Mold Shrinkage, Flow 0.017 cm/cm
0.017 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4 2577
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.0 MPa
8850 psi
ISO 527-1/-2
Elongation at Break 15 %
15 %
Nominal; ISO 527-1/-2
Elongation at Yield 8.0 %
8.0 %
ISO 527-1/-2
Tensile Modulus 2.80 GPa
406 ksi
ISO 527-1/-2
Flexural Modulus 2.70 GPa
392 ksi
ISO 178
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Melting Point 168 °C
334 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Part Marking Code >POM-MFe<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM-MFe