Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 383700 cP @Shear Rate 500 1/s, Temperature 240 °C |
383700 cP @Shear Rate 500 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |