Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.0 cP @Temperature 25.0 °C |
3.0 cP @Temperature 77.0 °F |
Uncured |
Permabond 930 Cyanoacrylate PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The .. |
|||
Viscosity | 3.0 cP @Temperature 40.0 °C |
3.0 cP @Temperature 104 °F |
|
Solvay AMGARD® DBBP Phosphorus Derivative Identification: DIBUTYL BUTYL PHOSPHONATECAS: 78 – 46 – 6Molecular formula: C12H27O3PAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: Organophosphorous comp.. |