Polymer Property : Viscosity = 3.0 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 3.0 cP

@Temperature 25.0 °C
3.0 cP

@Temperature 77.0 °F
Uncured
Permabond 930 Cyanoacrylate
PERMABOND 930 is a low odor, non­fogging, non­frosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The ..
Viscosity 3.0 cP

@Temperature 40.0 °C
3.0 cP

@Temperature 104 °F
Solvay AMGARD® DBBP Phosphorus Derivative
Identification: DIBUTYL BUTYL PHOSPHONATECAS: 78 – 46 – 6Molecular formula: C12H27O3PAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: Organophosphorous comp..