Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 293100 cP @Shear Rate 500 1/s, Temperature 250 °C |
293100 cP @Shear Rate 500 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |