Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 29000 cP @Temperature -25.0 °C |
29000 cP @Temperature -13.0 °F |
MRV; ASTM D4684 |
ExxonMobil Mobil Delvac 15W-40 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |
|||
Viscosity | 29000 cP @Shear Rate 1000 1/s, Temperature 190 °C |
29000 cP @Shear Rate 1000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2503 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with excellent rigidity. It h.. |
|||
Viscosity | 29000 cP @Temperature -25.0 °C |
29000 cP @Temperature -13.0 °F |
MRV; ASTM D4684 |
ExxonMobil Mobil Delvac 15W-40 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |