Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 29 cP @Temperature 30.0 °C |
29 cP @Temperature 86.0 °F |
10% wt, Toluene Solution |
Kuraray SEPTON® S2063 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Viscosity | 29 cP @Shear Rate 1000 1/s, Temperature 270 °C |
29 cP @Shear Rate 1000 1/s, Temperature 518 °F |
|
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |