Polymer Property : Viscosity = 28 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 28 cP

@Temperature 30.0 °C
28 cP

@Temperature 86.0 °F
5% wt Toluene Solution
Kuraray SEPTON® S2005 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
Viscosity 28 cP

@Temperature 180 °C
28 cP

@Temperature 356 °F
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate
Cyclics CBT® 200 Thermoplastic Resin
CBT® 200 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between..
Viscosity 28 cP

@Temperature 40.0 °C
28 cP

@Temperature 104 °F
Absolute
BASF Palatinol® N Diisononyl Phthalate
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl..