Physical Properties Metric English Comments
Viscosity 2520 cP

@Temperature 40.0 °C
2520 cP

@Temperature 104 °F
BASF Pluracol® 5250 Graft Slabstock Foam Polyol
Description: Pluracol® 5250 polyol is a graft polyether triol containing copolymerized styrene and acrylonitrile. This secondary hydroxyl-terminated polyol contains approximately 50% solids. It is ..