Viscosity 2300 cP

@Temperature 40.0 °C
2300 cP

@Temperature 104 °F
BASF Pluracol® 735 Rigid Polyol
Description: Pluracol® 735 polyol is a modifying polyol which can be used in a wide variety of rigid foam applications and can be formulated using crude MDI, crude TDI, or TDI quasi-prepolymers. Fo..