Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 22500 cP @Temperature 25.0 °C |
22500 cP @Temperature 77.0 °F |
ET500B, Amine Hardener |
Permabond ET500 Epoxy Resin PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera.. |