Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 220000 cP @Shear Rate 1000 1/s, Temperature 190 °C |
220000 cP @Shear Rate 1000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow HDPE 08454N High Density Polyethylene DOW HDPE 08454N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness, with good stiffness. This resin has good processability over a wi.. |