Physical Properties Metric English Comments
Viscosity 220000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
220000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow HDPE 08454N High Density Polyethylene
DOW HDPE 08454N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness, with good stiffness. This resin has good processability over a wi..