Polymer Property : Viscosity = 220 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 220 cP

@Shear Rate 10.0 1/s,
Temperature 290 °C
220 cP

@Shear Rate 10.0 1/s,
Temperature 554 °F
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY
Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Viscosity 220 cP

@Shear Rate 10.0 1/s,
Temperature 280 °C
220 cP

@Shear Rate 10.0 1/s,
Temperature 536 °F
Solvay TECHNYL® A 221 PA66, DRY
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
Viscosity 220 cP

@Shear Rate 100 1/s,
Temperature 270 °C
220 cP

@Shear Rate 100 1/s,
Temperature 518 °F
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY
Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i..
Viscosity 220 cP

@Shear Rate 1000 1/s,
Temperature 270 °C
220 cP

@Shear Rate 1000 1/s,
Temperature 518 °F
Solvay TECHNYL® C 536XT PA6, DRY
Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing..
Viscosity 220 cP

@Temperature 60.0 °C
220 cP

@Temperature 140 °F
BASF Pluracol® TP 4542 Specialty Polyol
Description: Pluracol® TPE 4542 polyol is a moderately high molecular weight polyether triol that can be used in polyurethane sealant applications, flexible integral skin foam and cold-cured foam a..