Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 21 cP @Shear Rate 10000 1/s, Temperature 290 °C |
21 cP @Shear Rate 10000 1/s, Temperature 554 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |