Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2.10e+6 cP

@Shear Rate 100 1/s,
Temperature 190 °C
2.10e+6 cP

@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Total Xsene® XS10 B HDPE, pipe, injection molding
FINATHENE® XS10 B is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS10 B is a high performance black compound speci..
Viscosity 2.10e+6 cP

@Shear Rate 100 1/s,
Temperature 190 °C
2.10e+6 cP

@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Total Xsene® XS10 H HDPE, pipe, injection molding
FINATHENE® XS 10 H is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 H is a high performance dark blue compound..
Viscosity 2.10e+6 cP

@Shear Rate 100 1/s,
Temperature 190 °C
2.10e+6 cP

@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Total Xsene® XS10 Orange YCF HDPE, pipe
FINATHENE® XS 10 ORANGE YCF is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 ORANGE YCF is a high performance ..