Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 190 cP @Shear Rate 100 1/s, Temperature 280 °C |
190 cP @Shear Rate 100 1/s, Temperature 536 °F |
shear rate: 100/s |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 190 cP @Shear Rate 1000 1/s, Temperature 250 °C |
190 cP @Shear Rate 1000 1/s, Temperature 482 °F |
|
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |