Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 185 cP @Shear Rate 1000 1/s, Temperature 230 °C |
185 cP @Shear Rate 1000 1/s, Temperature 446 °F |
Apparent viscosity; ASTM D3835 |
Huntsman Rexell® H2105 Injection Molding LLDPE
(discontinued **) Linear-low high density, injection molding, FDA compliant.Features: High impact strength with reasonable flow.Applications: Articles that must withstand long-term heavy loading such as bottle crates.. |
|||
Viscosity | 185 cP @Temperature 60.0 °C |
185 cP @Temperature 140 °F |
|
BASF Pluracol® 355 Specialty Polyol Description: Pluracol® 355 polyol is an amine-based tetrol of low equivalent weight with built-in catalytic activity. Because of its unusual behavior, this polyol has found wide application in flex.. |