Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1819 cP @Temperature 23.0 °C |
1819 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® ED1021 Epoxy Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Unique features include its abil.. |