Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5000 - 18000 cP @Temperature 25.0 °C |
5000 - 18000 cP @Temperature 77.0 °F |
E Curative |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Viscosity | 12000 - 18000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
12000 - 18000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2110309D5 Carbon Graphite Ink This is designed for screen-printing of working electrodes for electrochemical sensors. The paste is formulated to give superior printing properties with good definition for fine line printing.Produ.. |
|||
Viscosity | 15000 - 18000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
15000 - 18000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2070412D3 Polymer Dielectric Green colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The formulation .. |