Physical Properties Metric English Comments
Viscosity 162000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
162000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Versaflex™ CL E90 Thermoplastic Elastomer (TPE)
Versaflex™ CL E90 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E90 is also formulated without the use of plasticizer..