Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 162000 cP @Shear Rate 1340 1/s, Temperature 200 °C |
162000 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ CL E90 Thermoplastic Elastomer (TPE) Versaflex™ CL E90 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E90 is also formulated without the use of plasticizer.. |