Physical Properties Metric English Comments
Viscosity 149600 cP

@Shear Rate 500 1/s,
Temperature 280 °C
149600 cP

@Shear Rate 500 1/s,
Temperature 536 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Viscosity 149600 cP

@Shear Rate 500 1/s,
Temperature 280 °C
149600 cP

@Shear Rate 500 1/s,
Temperature 536 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers