Polymer Property : Viscosity = 14500 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 14500 cP

@Temperature 40.0 °C
14500 cP

@Temperature 104 °F
BASF Pluracol® 736 Rigid Polyol
Description: Pluracol® 736 polyol is an aromatic initiator-based polyol which can be used in a variety of rigid foam formulations. This polyol can be reacted with crude MDI, crude TDI or TDI quasip..