Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 14500 cP @Temperature 40.0 °C |
14500 cP @Temperature 104 °F |
|
BASF Pluracol® 736 Rigid Polyol Description: Pluracol® 736 polyol is an aromatic initiator-based polyol which can be used in a variety of rigid foam formulations. This polyol can be reacted with crude MDI, crude TDI or TDI quasip.. |