Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 142200 cP @Shear Rate 5000 1/s, Temperature 250 °C |
142200 cP @Shear Rate 5000 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |