Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 130500 cP @Shear Rate 500 1/s, Temperature 295 °C |
130500 cP @Shear Rate 500 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Viscosity | 130500 cP @Shear Rate 5000 1/s, Temperature 260 °C |
130500 cP @Shear Rate 5000 1/s, Temperature 500 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |