Polymer Property : Viscosity = 12500 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 12500 cP

@Shear Rate 100000 1/s,
Temperature 270 °C
12500 cP

@Shear Rate 100000 1/s,
Temperature 518 °F
DSM Arnite® TV4 441 (PBT+PET)-GF20
20% Glass Reinforced
Viscosity 12500 cP

@Shear Rate 100000 1/s,
Temperature 270 °C
12500 cP

@Shear Rate 100000 1/s,
Temperature 518 °F
DSM Arnite® TV4 461 (PBT+PET)-GF30
30% Glass Reinforced
Viscosity 12500 cP

@Shear Rate 100000 1/s,
Temperature 310 °C
12500 cP

@Shear Rate 100000 1/s,
Temperature 590 °F
DSM Arnite® AV2 370 HF PET-GF35
35% Glass Reinforced, Brake Booster Body Valves, High Flow
Viscosity 12500 cP

@Shear Rate 100000 1/s,
Temperature 270 °C
12500 cP

@Shear Rate 100000 1/s,
Temperature 518 °F
DSM Arnite® T06 202 /A PBT
Medium Viscosity, Injection Molding
Viscosity 12500 - 250000 cP

@Temperature 270 - 310 °C
12500 - 250000 cP

@Temperature 518 - 590 °F
Average value: 96700 cP Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Viscosity 12500 - 250000 cP

@Shear Rate 100 - 100000 1/s
12500 - 250000 cP

@Shear Rate 100 - 100000 1/s
Average value: 96700 cP Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Viscosity 12500 cP

@Temperature 25.0 °C
12500 cP

@Temperature 77.0 °F
Lendell Manufacturing Prepol Pre Polymer
Liquid Apperance, Amber, honey likePolyether Polyurethane Pre-Polymer is water activated, yielding foams and gels with unique characteristics - Hydrophilic, Bio-Compatible, loading of additives to 8..