Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 113400 cP @Shear Rate 5000 1/s, Temperature 280 °C |
113400 cP @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |