Polymer Property : Viscosity = 107100 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 107100 cP

@Shear Rate 5000 1/s,
Temperature 200 °C
107100 cP

@Shear Rate 5000 1/s,
Temperature 392 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..
Viscosity 107100 cP

@Shear Rate 5000 1/s,
Temperature 200 °C
107100 cP

@Shear Rate 5000 1/s,
Temperature 392 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical ..