Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 107 cP @Shear Rate 100 1/s, Temperature 270 °C |
107 cP @Shear Rate 100 1/s, Temperature 518 °F |
|
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |