Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 103100 cP @Shear Rate 500 1/s, Temperature 305 °C |
103100 cP @Shear Rate 500 1/s, Temperature 581 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |