Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 102722 - 460190 cP @Temperature 240 - 260 °C |
102722 - 460190 cP @Temperature 464 - 500 °F |
Average value: 234000 cP Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Viscosity | 102722 - 460190 cP @Shear Rate 500 - 5000 1/s |
102722 - 460190 cP @Shear Rate 500 - 5000 1/s |
Average value: 234000 cP Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |