Polymer Property : Viscosity = 102722 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 102722 - 460190 cP

@Temperature 240 - 260 °C
102722 - 460190 cP

@Temperature 464 - 500 °F
Average value: 234000 cP Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Viscosity 102722 - 460190 cP

@Shear Rate 500 - 5000 1/s
102722 - 460190 cP

@Shear Rate 500 - 5000 1/s
Average value: 234000 cP Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..