Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.76 cP @Temperature 50.0 °C |
0.76 cP @Temperature 122 °F |
|
Solvay Chemicals Epichlorohydrin Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy appli.. |
|||
Viscosity | 0.76 cP @Temperature 35.0 °C |
0.76 cP @Temperature 95.0 °F |
Dynamic |
Solvay Chemicals Perchloroethylene Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay |