Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.44 cP @Temperature 302 °C |
0.44 cP @Temperature 575 °F |
|
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |
|||
Viscosity | 0.44 cP @Temperature 110 °C |
0.44 cP @Temperature 230 °F |
|
Solvay Chemicals Epichlorohydrin Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy appli.. |
|||
Viscosity | 0.44 cP @Temperature 100 °C |
0.44 cP @Temperature 212 °F |
Dynamic |
Solvay Chemicals Perchloroethylene Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay |