Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 7.9 cSt | 7.9 cSt | ASTM D445 |
ExxonMobil 825 Mobil SHC 800 Series Mobil SHC 800 Series turbine oils are designed specifically to meet the needs of the most severe industrial gas turbine applications with a nominal 10,000 hour TOST life. They are recommended for th.. |
|||
Kinematic Viscosity at 100°C (212°F) | 7.9 cSt | 7.9 cSt | ASTM D445 |
ChevronTexaco Elite-Cut® AXH Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Kinematic Viscosity at 100°C (212°F) | 7.9 cSt | 7.9 cSt | ASTM D445 |
ChevronTexaco FM ISO 46 Synthetic Compressor Oil FeaturesChevron Synthetic Compressor Oil FM is a PAO based, synthetic, food grade, compressor oil.Although Chevron Synthetic Compressor Oil FM offers a reduced risk of fires and explosions, it is no.. |
|||
Kinematic Viscosity at 100°C (212°F) | 7.9 cSt | 7.9 cSt | ASTM D445 |
ExxonMobil 625 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Kinematic Viscosity at 100°C (212°F) | 7.9 cSt | 7.9 cSt | ASTM D445 |
ExxonMobil 825 Mobil SHC 800 Series Mobil SHC 800 Series turbine oils are designed specifically to meet the needs of the most severe industrial gas turbine applications with a nominal 10,000 hour TOST life. They are recommended for th.. |
|||
Kinematic Viscosity at 100°C (212°F) | 7.9 cSt | 7.9 cSt | ASTM D445 |
ExxonMobil 625 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |