Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco FM ISO 46 Synthetic Compressor Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name FM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco FM ISO 46 Synthetic Compressor Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Synthetic Compressor Oil FM is a PAO based, synthetic, food grade, compressor oil.Although Chevron Synthetic Compressor Oil FM offers a reduced risk of fires and explosions, it is not a fire-resistant fluid.ApplicationsChevron Synthetic Compressor Oil FM is recommended for both rotary and reciprocating air compressors. It is particularly useful in applications where incidental food contact may occur with oil in the discharge air.Chevron Synthetic Compressor Oil FM may also be used where an R&O or mild antiwear hydraulic oil with high temperature stability and excellent low temperature fluidity performances are required.Chevron Synthetic Compressor Oil FM is fully compatible in ammonia refrigerant systems as well as systems containing R 12 refrigerant. Chevron Synthetic Compressor Oil FM is not compatible with HFC-134A type refrigerant.Chevron Synthetic Compressor Oil FM is similar to mineral oil in its compatibility with paints, seals, gaskets and hoses. Some examples of commonly used materials are1: , Delrin, epoxy paint, high nitrile Buna N, nylon, oil-resistant alkyd, PBT, Teflon, and Viton.
Physical Properties Metric English Comments
Specific Gravity 0.840 g/cc
0.840 g/cc
API Gravity 36.9 °
36.9 °
Viscosity Measurement 135
135
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 244 SUS
244 SUS
Saybolt Viscosity at 210°F 53 SUS
53 SUS
Kinematic Viscosity at 40°C (104°F) 47.8 cSt
47.8 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 7.9 cSt
7.9 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Wear 0.400 mm
0.0157 in
Thermal Properties Metric English Comments
Pour Point -57.0 °C
-70.6 °F
ASTM D97
Flammability Test 380
380
Autoignition Point, °C
Flash Point 240 °C
464 °F
ASTM D92
Descriptive Properties Value Comments
Demulsibility at 54°C, mL 40-40-0
Foaming Tendency Sequence I Nil
Foaming Tendency Sequence II Nil
Foaming Tendency Sequence III Nil
Rust preventative Test Procedure B Pass
Synthetic Sea Water
Rust Procedure A, Distilled Water Pass