Kinematic Viscosity at 100°C (212°F) 18.5 cSt
18.5 cSt
ChevronTexaco Aries® 220
Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w..
Kinematic Viscosity at 100°C (212°F) 18.5 cSt
18.5 cSt
ConocoPhillips 100 FR Hydraulic Fluid ISO
Description: Conoco FR Hydraulic Fluid is a fire-resistant, water-in-oil, invert-emulsion fluid for hydraulic systems, such as those found in underground mining equipment in which fire hazard and pe..
Kinematic Viscosity at 100°C (212°F) 18.5 cSt
18.5 cSt
ConocoPhillips Hydroclear® 220 Wet Gas Compressor Fluid ISO 220
Description: Conoco Hydroclear® Wet Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality, hydrocracked base oil..
Kinematic Viscosity at 100°C (212°F) 18.5 cSt
18.5 cSt
ASTM D445
ChevronTexaco ISO 220 Cylinder Oil W
FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal..