Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 15.4 cSt | 15.4 cSt | |
ChevronTexaco 17 MG 2000 Diesel Engine Oil Texaco Diesel Engine Oils deliver value through:Ability to maximize oil and filter lifeImproved wear controlExtended drainsExtends oil drains in new low oil consumption GE locomotives, reducing oil .. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.4 cSt | 15.4 cSt | ASTM D445 |
ChevronTexaco Delo® 477 CFO Marine Engine Oil, SAE 20W-40 FeaturesChevron Marine Engine Oils Delo 477 CFO are superior high dispersancy, high alkalinity, 17 base Number engine oils.They are manufactured using the highest quality paraffinic base oils, a non.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.4 cSt | 15.4 cSt | ASTM D445 |
ChevronTexaco Delo® 6170 CFO Diesel Engine Oil, SAE 20W-40 FeaturesChevron Diesel Engine Oils Delo 6170 CFO are outstanding high dispersancy, high alkalinity, 17 base number engine oils for use in diesel engines used in railroad, power generation, oil well .. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.4 cSt | 15.4 cSt | ASTM D445 |
ChevronTexaco FM Seamer Oil FeaturesChevron Seamer Oil FM is a premium performance industrial lubricant designed specifically to be used in Angelus Sanitary Can Machine Company seaming equipment and other similar applications... |
|||
Kinematic Viscosity at 100°C (212°F) | 15.4 cSt | 15.4 cSt | |
ChevronTexaco URSA® SAE 15W-40 Premium TDX Texaco Ursa Premium TDX SAE 15W-40 delivers value through:Reduced wear — Prolonging component life and providing reduced maintenance costs.Improved engine cleanliness — Providing efficient operati.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.4 cSt | 15.4 cSt | |
ChevronTexaco URSA® SAE 15W-40 Super Plus Texaco Ursa Super Plus SAE 15W-40 delivers value through:One oil for all services, both diesel and gasoline, minimizes the chance of misapplication.educed inventory investment — No need to maintain.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.4 cSt | 15.4 cSt | |
ConocoPhillips HD Fleet Supreme™ 15W-40 Engine Oil Description: Conoco HD Fleet Supreme Engine Oil is a high-quality engine oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. It easily satisfies the warr.. |