Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 13.7 cSt | 13.7 cSt | ASTM D445 |
ExxonMobil Gargoyle Arctic 228 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.7 cSt | 13.7 cSt | |
ExxonMobil Mobil 1 Racing 2T Motorcycle Oil 2-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.7 cSt | 13.7 cSt | ASTM D445 |
ExxonMobil Mobil Pegasus 15W-40 40 Mobil Pegasus Special is a high quality SAE 15W-40 gas engine oil primarily intended for the lubrication of crankcases and power cylinders of spark-ignited two- and four-cycle gas-fueled engines. It.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.7 cSt | 13.7 cSt | |
ChevronTexaco 150 PMO Premium Texaco PMO Premium oils deliver value through:Minimized unscheduled downtime — High oxidation stability provides excellent resistance to deposit formation. The detergent/dispersant additive system .. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.7 cSt | 13.7 cSt | ASTM D445 |
ChevronTexaco Supreme SAE 5W-40 Synthetic Motor Oil FeaturesChevron Supreme 100% Synthetic Motor Oils are designed for those drivers who demand the ultimate in engine protection. They provide an extra measure of protection for the investment in a spo.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.7 cSt | 13.7 cSt | ASTM D445 |
ExxonMobil Gargoyle Arctic 228 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.7 cSt | 13.7 cSt | |
ExxonMobil Mobil 1 Racing 2T Motorcycle Oil 2-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.7 cSt | 13.7 cSt | ASTM D445 |
ExxonMobil Mobil Pegasus 15W-40 40 Mobil Pegasus Special is a high quality SAE 15W-40 gas engine oil primarily intended for the lubrication of crankcases and power cylinders of spark-ignited two- and four-cycle gas-fueled engines. It.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.7 cSt | 13.7 cSt | |
ChevronTexaco Havoline® SAE 5W-40 Synthetic Motor Oil Havoline Synthetic Motor Oil is recommended for all four-stroke gasoline engines used in passenger cars, sport utility vehicles, and light trucks. 5W-40 meets: API Service Categories SL/CF, SJ/CFAC.. |