Material Notes:
Havoline Synthetic Motor Oil is recommended for all four-stroke gasoline engines used in passenger cars, sport utility vehicles, and light trucks. 5W-40 meets: API Service Categories SL/CF, SJ/CFACEA A3/B3BMW Longlife 98Mercedes Benz 229.1PorscheVolkswagen 502.00 and 505.00Volvo SMB 22-3Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 222100; MSDS Number: 8602
Physical Properties Metric English Comments
API Gravity 32.8 °
32.8 °
Viscosity 5000 cP

@Temperature -30.0 °C
5000 cP

@Temperature -22.0 °F
Cold Crank
Viscosity Measurement 158
158
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 87.7 cSt
87.7 cSt
Kinematic Viscosity at 100°C (212°F) 13.7 cSt
13.7 cSt
Ash 1.2 %
1.2 %
Sulfated Ash
Thermal Properties Metric English Comments
Pour Point -51.0 °C
-59.8 °F
Flash Point 222 °C
432 °F
Component Elements Properties Metric English Comments
Phosphorous, P 0.098 %
0.098 %
Zinc, Zn 0.103 %
0.103 %
Chemical Properties Metric English Comments
Total Base Number 8.8
8.8
ASTM D2896
Descriptive Properties Value Comments
Noack Volatility, wt% 8
250°C, 1 h
Users viewing this material also viewed the following: