Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 875 cSt | 875 cSt | See Note 3. |
ChevronTexaco Texclad® 2 Texaco Texclad 2 delivers value through:Water tolerance — Resists washout, even when subject to gross water contamination.Excellent adhesiveness — Assures good film strength even in a wet environm.. |