ChevronTexaco Texclad® 2

Category Fluid , Lubricant , Calcium Gellant
Manufacturer ChevronTexaco Corp
Trade Name Texclad®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Texclad® 2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Texclad 2 delivers value through:Water tolerance — Resists washout, even when subject to gross water contamination.Excellent adhesiveness — Assures good film strength even in a wet environment.Texaco Texclad 2 is calcium-based grease, which contains special functional fillers such as molybdenum disulfide and graphite, which impart a long-lasting film on working surfaces. Texclad has good load carrying capability and is very resistant to water washout.Texaco Texclad 2 additive system includes friction modifiers such as molybdenum disulfide and graphite, which apply a long lasting antiwear film on lubricated surfaces.Texaco Texclad 2 is recommended:For ball mill gears, traveling water screens, and fork lifts.For chain and sprocket lubrication and as a tenacious fifth wheel lubricant.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.CPS Number: 221956; MSDS Number: 9008
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 875 cSt
875 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 36.5 cSt
36.5 cSt
See Note 3.
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 280
280
Unknown Amount of Work, 25°C (77°F)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 79.0 °C
174 °F
See Note 2.
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
See Note 1.
Dropping Point 232 °C
450 °F
Descriptive Properties Value Comments
Color Black
Texture Tacky
Thickener, % 9
Calcium